<原著>火炎溶射法によるレジン前装冠への応用 : 至適溶射条件の検討
https://hsuh.repo.nii.ac.jp/records/7623
https://hsuh.repo.nii.ac.jp/records/7623671c5e57-b1be-4fab-9590-b7afaa39f1b4
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 紀要論文(ELS) / Departmental Bulletin Paper(ELS)(1) | |||||
---|---|---|---|---|---|---|
公開日 | 1991-06-30 | |||||
タイトル | ||||||
タイトル | <原著>火炎溶射法によるレジン前装冠への応用 : 至適溶射条件の検討 | |||||
言語 | ja | |||||
タイトル | ||||||
タイトル | <ORIGINAL ARTICLE>Application of Flame Spray Method to Resin Veneered Crown : An Investigation of Adhesion on the Most Suitable Spraying Condition | |||||
言語 | en | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
主題 | flame spray | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
主題 | spraying distance | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
主題 | spraying powder | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
主題 | resin-bonded. | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | departmental bulletin paper | |||||
ページ属性 | ||||||
内容記述タイプ | Other | |||||
内容記述 | P(論文) | |||||
言語 | ja | |||||
著者名(日) |
井上, 龍一郎
× 井上, 龍一郎× 坂口, 邦彦× 日景, 盛× 澤田, 教彰× 越智, 守生× 広瀬, 由紀人× 伊藤, 仁× 小林, 秀樹 |
|||||
著者所属(日) | ||||||
ja | ||||||
東日本学園大学歯学部歯科補綴学第Ⅱ講座 | ||||||
著者所属(英) | ||||||
en | ||||||
Department of Crown and Bridge Prosthodontics, School of Dentistry, HIGASHI-NIPPON-GAKUEN UNIVERSITY | ||||||
抄録(英) | ||||||
内容記述タイプ | Other | |||||
内容記述 | The shear bond strength of 12% Au-Ag-Pd alloy, when a flame spraying treatment was applied on the surface of it, working on 4-META/MMA-TBB opaque resin was compared with that of retention beads SSR. And the most suitable distance for each spraying powder was evaluated by compressive shear tests. The results of these tests indicated the following: 1. 442 sprayed at a distance directed by the maker had a significant strength by a higher average than retention beads SSR. 2. 442, 443 sprayed at a distance of 25 cm and 447, 43C sprayed at a distance of 20 cm showed the highest bond strength among those spraying distances (10cm, 15cm, 20cm, 25cm). 3. 442 sprayed at 20 cm and 25 cm had a significant bond strength by a higher average than retention beads SSR. 4. The shear bond strength at a distance of 10 cm had a tendency for every powder to lower. 5. A spraying distance of high shear bond strength was indicated between 20cm and 25cm at all spraying powders. | |||||